Standard Test Methods of Polyurethane Raw Materials: Determination of the Polymerized Ethylene Oxide Content of Polyether Polyols
1.1 Test Method A—Proton Nuclear Magnetic Resonance Spectroscopy (1H NMR) measures polymerized ethylene oxide (EO) content of ethylene oxide (EO) propylene oxide (PO) polyether polyols used in flexible polyurethane foams and non-foams. It is suitable for diols initiated from glycols of EO or PO containing EO percentages >5. For triols initiated with glycerol (glycerin) and trimethylolpropane, an uncorrected EO value is obtained since both initiators have protons that contribute to the EO measurement.
1.2 Test Method B—Carbon-13 Nuclear Magnetic Resonance Spectroscopy (13C NMR) measures the polymerized EO content of EO-PO polyether polyols used in flexible polyurethane foams and non-foams. It is suitable for diols and triols made from the commonly used initiators and containing EO percentages >5.
1.3 The values stated in SI units are to be regarded as standard.
1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.
Note 1: There is no known ISO equivalent to this standard.
1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International StandardDetails, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.