Standard Test Method for Polyurethane Raw Materials: Determination of Acidity in Moderate to High Acidity Aromatic Isocyanates
1.1 This test method determines the acidity, expressed as parts per million (ppm) of HCl, in aromatic isocyanate samples of greater than 100–ppm acidity. The test method is applicable to products derived from toluene diisocyanate and methylene-bis-(4–phenylisocyanate) (see Note 1).
Note 1: This test method is equivalent to ISO 14898, Test Method A.
1.2 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International StandardDetails, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.