Standard Practice for Evaluating Stress-Corrosion Cracking Resistance of Low Copper 7XXX Series Al-Zn-Mg-Cu Alloys in Boiling 6% Sodium Chloride Solution

Standard Details

1.1 This stress corrosion practice is intended for statically loaded smooth non-welded or welded specimen tests of 7XXX series Al-Zn-Mg alloys containing less than 0.26% copper.

1.2 This practice is concerned primarily with the test medium which may be used with a variety of test specimens and methods for applying stress. Exposure times, criteria of failure, and so on, are variable and not specified.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. See Section 8 for additional precautions.

General Information

Status : Historical
Standard Type: Main
Document No: ASTM G103 : 97
Document Year: 1997
Pages: 3
  • Section Volume:
  • 03.02 Volume 03.02 Corrosion of Metals; Wear and Erosion

Life Cycle

Currently Viewing

Historical
ASTM G103 : 97
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2024 BSB Edge Private Limited.

Enquire now +