Standard Classification of Resistance to Stress-Corrosion Cracking of Heat-Treatable Aluminum Alloys

Standard Details

1.1 This classification covers alphabetical ratings of the relative resistance to SCC of various mill product forms of the wrought 2XXX, 6XXX, and 7XXX series heat-treated aluminum alloys and the procedure for determining the ratings.

1.2 The ratings do not apply to metal in which the metallurgical structure has been altered by welding, forming, or other fabrication processes.

1.3 The values stated in SI units are to be regarded as standard. The values given in parentheses after SI units are provided for information only and are not considered standard.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International StandardDetails, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

General Information

Status : ACTIVE
Standard Type: Main
Document No: ASTM G64 : 99(2021)
Document Year: 1999
Pages: 4
  • Section Volume:
  • 03.02 Volume 03.02 Corrosion of Metals; Wear and Erosion

Life Cycle

Currently Viewing

ACTIVE
ASTM G64 : 99(2021)

Historical
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2024 BSB Edge Private Limited.

Enquire now +