Standard Classification of Resistance to Stress-Corrosion Cracking of Heat-Treatable Aluminum Alloys

Standard Details

1.1 This standard contains alphabetical ratings of the relative resistance to SCC of various mill product forms of the wrought 2XXX, 6XXX, and 7XXX series heat-treated aluminum alloys and the procedure for determining the ratings.

1.2 The ratings do not apply to metal in which the metallurgical structure has been altered by welding, forming, or other fabrication processes.