ISO 15609-5:2011 specifies requirements for the content of welding procedure specifications for resistance spot, seam, butt and projection welding processes. It is necessary to establish the acceptability of applying the principles of ISO 15609-5:2011 to other resistance and related welding processes before any qualification is undertaken.

Variables listed in ISO 15609-5:2011 are those influencing either weld dimensions (quality), weld nugget dimension, weld pattern positioning, mechanical properties or geometry of the welded joint.

General Information

Status : Published
Standard Type: Main
Document No: ISO 15609-5:2011
Document Year: 2011
Pages: 13
Edition: 2
  • Section Volume:
  • ISO/TC 44/SC 6. Resistance welding and allied mechanical joining

Life Cycle

Currently Viewing

Published
ISO 15609-5:2011
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2024 BSB Edge Private Limited.

Enquire now +