Corrosion of metals and alloys — Stress corrosion testing — Part 3: Preparation and use of U-bend specimens

Standard Details

Covers procedures for designing, preparing and using U-bend test specimens. These specimens may be used to test a variety of product forms (for example sheet, plate, flat extruded material, wire or rod). The principal acvantages of the U-bend test are its simplicity and its adaptability for use in plants. A disadvantage is that stesses cannot be quantified with accuracy. U-bend specimens made from high strength materials may fracture rapidly and can be dangerous.

General Information

Status : Published
Standard Type: Main
Document No: ISO 7539-3:1989
Document Year: 1989
Pages: 3
Edition: 1
  • Section Volume:
  • ISO/TC 156. Corrosion of metals and alloys
  • ICS:
  • 77.060 Corrosion of metals

Life Cycle

Currently Viewing

Published
ISO 7539-3:1989
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2024 BSB Edge Private Limited.

Enquire now +