Corrosion of metals and alloys — Evaluation of stress corrosion cracking by the drop evaporation test

Standard Details

1.1 This International Standard specifies the procedure for determining the relative resistance of stainless steels

and nickel-base alloys to stress corrosion cracking in a sodium chloride drop evaporation system.

1.2 The method results in a threshold stress to fracture, the magnitude of which can be used to rank the relative

performance of different alloys for this environment.

General Information

Status : Published
Standard Type: Main
Document No: ISO 15324:2000
Document Year: 2000
Pages: 9
Edition: 1
  • Section Volume:
  • ISO/TC 156. Corrosion of metals and alloys
  • ICS:
  • 77.060 Corrosion of metals

Life Cycle

Currently Viewing

Published
ISO 15324:2000
Knowledge Corner

Expand Your Knowledge and Unlock Your Learning Potential - Your One-Stop Source for Information!

© Copyright 2024 BSB Edge Private Limited.

Enquire now +