BS ISO 18177 Plastics - Test method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymers by differential scanning calorimetry (DSC)

General Information

Status : Definitive
Standard Type: Main
Document No: 24/30463784 DC
Document Year: 16
Pages: 29
  • Section Volume:
  • GBM45 Plastics Industry (GMB45)